[TheForge] Gas Forge Recommendation
Rick
rick at smokyforge.com
Tue Jul 12 12:45:53 EDT 2005
Not MY site, but the photo access site listed at the bottom of each theForge
message. That is the site with the ceramic chip pictures on it. ( In the
forge section)
Rick
----- Original Message -----
From: "don schad" <sir.eggplantalot at gmail.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, July 12, 2005 11:38 AM
Subject: Re: [TheForge] Gas Forge Recommendation
Can you send a link? I looked on www.smokyforge.com but I couldn't
find any picture site with forges listed (just two galleries). Is it
a different site?
Thanks,
don
On 7/12/05, Rick <rick at smokyforge.com> wrote:
> Some one put some pics of a ceramic chip forge on our picture site under
> forges. I would like to know who made the one in the pictures as I cannot
> even remember who posted it. But the pics are there.
>
> Rick Crawford at Rafter Lazy C
> Home of Smoky Forge and Lem the Wonder Mule
> In the middle of Northern Illinois
>
> http://www.smokyforge.com
> rick at smokyforge.com
>
>
> ----- Original Message -----
> From: <Keporter at aol.com>
> To: <theforge at mailman.qth.net>
> Sent: Tuesday, July 12, 2005 10:38 AM
> Subject: Re: [TheForge] Gas Forge Recommendation
>
>
> >
> >
> > In a message dated 7/11/2005 6:55:15 P.M. Pacific Standard Time,
> > robi5515 at bellsouth.net writes:
> >
> > Hey Mike,
> > Do you have a picture or better yet a diagram of a ceramic chip forge.
> > I'm having a hard time visualizing it.
> > Chuck
> >
> >
> > Chuck
> > There isn't very much to visualize. Just think about the construction
> > of
> > a
> > regular coal fired forge, replacing the coal with broken refractory
> > brick
> > (home made ceramic balls of castable refractory are better), change out
> > the
> > tuyer for a refractory portal and gas burner, and then make a few other
> > changes,
> > like making the forge body out of heavy kiln shelving (or castable
> > refractory) in order to take the heat, and your in business. You can
> > find
> > photos of
> > ceramic chip forges on the Flamefast UK site, but they won't tell you
> > all
> > that
> > much. You can also find diagrams of ceramic ball furnaces on English
> > and
> > German sites. The central principle in both uses is the same; hot gases
> > rise, but
> > when they rise through ceramic refractory chunks, a lot more of their
> > heat
> > remains behind. It is sort of the best of both worlds--coal fired, and
> > gas
> > fired. When turned down low, the forge can act as a brazing hearth,
> > providing
> > secondary heat for gas welding.
> > Is this design the be-all and end-all of forges? There ain't no such
> > animal.
> > Wishing for the ultimate forge, or torch, or furnace is a classic trap,
> > confining imagination in a closed loop. It is better to spend a little
> > time
> > studying the underlying principles, and build two or three different
> > forges for
> > different tasks. This will become a necessity as fuel prices continue
> > to
> > climb.
> >
> > I will be building such a forge as part of the hot-work station for
> > book
> > two
> > this winter
> > Mike P.
> >
> > My email address is changing to keporter. at comcast.net effective
> > 7/15/05
>
>
>
> --
> No virus found in this outgoing message.
> Checked by AVG Anti-Virus.
> Version: 7.0.323 / Virus Database: 267.8.11/45 - Release Date: 7/9/2005
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--
No virus found in this incoming message.
Checked by AVG Anti-Virus.
Version: 7.0.323 / Virus Database: 267.8.11/45 - Release Date: 7/9/2005
--
No virus found in this outgoing message.
Checked by AVG Anti-Virus.
Version: 7.0.323 / Virus Database: 267.8.11/45 - Release Date: 7/9/2005
More information about the TheForge
mailing list