[TheForge] press vs power hammer

Bowie-- Ron Claiborne bowie2002 at comcast.net
Fri Jan 21 09:18:58 EST 2005


i have listed a few pictures and links so that you that are interested in 
powder or building Damascus and in using a press you may get a better idea 
of the process and the machine used these are press that i have built 
forgive me


>this is a link for the most part are knife makers but its talking about 
>lots of stuff dealing with process and tools as 
>http://www.knifenetwork.com/forum/forumdisplay.php?f=76

http://www.knifenetwork.com/forum/attachment.php?attachmentid=70

http://www.knifenetwork.com/forum/showpost.php?p=134725&postcount=39

http://www.fibermascus.com/yellowpress.jpg

http://www.fibermascus.com/yellowdies.jpg

http://www.knifenetwork.com/forum/showthread.php?t=23022

http://www.knifenetwork.com/forum/showpost.php?p=161949&postcount=1

http://www.knifenetwork.com/forum/showpost.php?p=142870&postcount=1