[TheForge] press vs power hammer
Phil
mobjak at yahoo.com
Fri Jan 21 06:54:28 EST 2005
Lon:
I've seen two of these hammers in use, and IMHO they
are not worth building. For the same time spent
building a rusty or a dusty, you could build a kinyon
style air hammer that would hit harder with more
control.
Phil
--- Lon Humphrey <ironcrossforge at adelphia.net> wrote:
> ok so what do you all think about the hammer that
> the appaclation
> blacksmiths built rusty or dusty
> http://www.appaltree.net/rusty/super_rusty.htm
>
> just wondering how well it holds up over time
> ----- Original Message -----
> From: "John Switzer" <switz at mindspring.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Thursday, January 20, 2005 7:13 PM
> Subject: Re: [TheForge] press vs power hammer
>
>
> >A press is a great tool for bending and contouring
> stock to shape, but for
> >general forging I would go with the power hammer.
> I do have a fly press
> >and love it, I just think if you can only have one
> or the other most people
> >would get more use from a power hammer.
> >
> > John
> >
> >
> >>hello, i have a question on wheather to build a
> power hammer or a
> >>hydhaulic press. the hammer in question would be
> dusty or rusty from one
> >>of the abana groups.
> >>or would my money be better spent in turning the
> log splitter into a
> >>press. i do alot of knife work but i do dink
> around with ornimental stuff
> >>too
> >>
> >>_______________________________________________
> >>Manage membership or unsubscribe at:
> >>http://mailman.qth.net/mailman/listinfo/theforge
> >>theforge mail list group photo site is
> >>http://www.photoaccess.com
> >>Login: blacksmithblacksmith at hotmail.com
> >>password: anvil
> >>___________
> >>
> >>
> >
> > John Switzer
> > 7019 Burnt Mill Rd
> > Beulah, CO 81023
> > (719) 485-3109
> >
> >
> >
> > _______________________________________________
> > Manage membership or unsubscribe at:
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: blacksmithblacksmith at hotmail.com
> > password: anvil
> > ___________
> >
> >
> >
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
__________________________________
Do you Yahoo!?
All your favorites on one personal page Try My Yahoo!
http://my.yahoo.com
More information about the TheForge
mailing list