  -Once it was soft enough to file, I left it that way.  Um, why would
  -one harden a ring?

Dunno, what kinda barroom brawls go on in the Great white North?  Suppose it
would keep it from getting scored/scratched by wrenches, knives, soup spoons
and dessert forks.

Kevin

  ------Original Message-----
  -From: theforge-bounces at mailman.qth.net
  -[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Mike Spencer
  -Sent: Saturday, January 15, 2005 1:50 AM
  -To: theforge at mailman.qth.net
  -Subject: [TheForge] Air-hardening Damascus (Was:: For the Rube Gold...)
  -
  -
  -
  -> With that VW/MS ring you made, did you leave it wood coal/annealed? or
  -> harden it any?
  -
  -Once it was soft enough to file, I left it that way.  Um, why would
  -one harden a ring?
  -
  -Regrettably, it got lost somewhere.  I keep thinking it'll turn up in
  -a box of miscellany or a floor crack.  I should do it over, eh?
  -
  -- Mike
  -
  ---
  -Michael Spencer                  Nova Scotia, Canada       .~.
  -                                                           /V\
  -mspencer at tallships.ca                                     /( )\
  -http://home.tallships.ca/mspencer/                        ^^-^^
  -
  ---
  -
  -
  -_______________________________________________
  -Manage membership or unsubscribe at:
  -http://mailman.qth.net/mailman/listinfo/theforge
  -theforge mail list group photo site is
  -http://www.photoaccess.com
  -Login:  blacksmithblacksmith at hotmail.com
  -password:  anvil
  -___________
  -
  -
  -
  -



More information about the TheForge mailing list