That explains how they bonded the steel to aluminum. Could make the base
out of some nice wood too, instead of aluminum. Oh, that has been done --
they call them stake anvils.
Dave
----- Original Message -----
From: "Dan Tull" <dantull at numail.org>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Monday, January 10, 2005 10:17 PM
Subject: Re: [TheForge] Re: Anvils
> Dave,
> Not only were they steel over al. , but there was a rubber spacer.
> dan tull
> georgia
> abba, afc, S.C. psba, obg,sofa
> ----- Original Message -----
> From: "David E. Smucker" <davesmucker at hotmail.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Monday, January 10, 2005 9:16 PM
> Subject: Re: [TheForge] Re: Anvils
>
>
>> Interesting -- I have never heard of an anvil made part out of aluminum
>> (wonder metal) and steel. Not sure why other than if is for ease of
>> movement. From my view point aluminum has neither the mass nor stiffness
>> required for a really good anvil. But from what you say with a steel
>> face and has good rebound. Is the horn steel or aluminum ? Some of the
>> aerospace alloys have lots of strength but bounding them to steel is not
>> easy. It can be done as either a friction weld or rolling mill forge
>> weld. (Maybe explosive too but I have never seen that my self.) If I was
>> going to try to make a composite aluminum steel anvil I would first roll
>> bond (rolling mill forge weld) steel to an aluminum substrate and then
>> weld the aluminum to the rest of the anvil. How was this one was made?
>> Cast aluminum base into a dovetailed steel face?
>>
>> In Alcoa we used to call aluminum the wonder metal -- "I wonder what it
>> is good for besides beer cans and airplanes?" But hey, they pay my
>> pension. And yes it has many many other good uses.
>>
>> Dave Smucker
>> ----- Original Message -----
>> From: <LrdThorolf at aol.com>
>> To: <theforge at mailman.qth.net>
>> Sent: Monday, January 10, 2005 8:18 PM
>> Subject: [TheForge] Re: Anvils
>>
>>
>>> Another thing about my anvil. When I got it, the horn had a real sharp
>>> point
>>> on it and walking around it would sometimes catch my leg and leave a
>>> nasty
>>> little cut on it. I ground about a half inch off of it, and it quit
>>> biting
>>> me. I have a Delta Future 2. Half steel and half Aluminum. Very little
>>> ring
>>> and a face that if you miss you had better be moving head out of the
>>> way. It
>>> weighs 100 pounds but has the size of most 150 to 200 pounders.
>>>
>>> Later Ike
>>> Pan's Forge
>>>
>>> But I love the heat. Just want it from the Forge. 4 seasons for me
>>> now.
>>>
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> password: anvil
>>> ___________
>>>
>>>
>>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list