[TheForge] Forge Welding Chainsaw Chain
Ralph Douglass
douglass at ptdcs2.ra.intel.com
Tue Jan 4 19:23:09 EST 2005
Andrew Vida wrote:
>
> Ralph Douglass wrote:
>
> > I am too lazy for that much work for marginal effect. Anyhoo the biggest
> > difference is how much 20 Mule foams when you put it on. BUt if you put
> > the borax on a a lower red color it will just melt and not bubble off.
> > At least my borax works this way.
>
> That's what I do. At cherry red, there is no foaming worth noting.
Andy!
How are you doing!?
I am doing better. But the drug therapy is a killer. But I am glad it
was not chemo.
Either way between the RAD treatments and all I was pretty physically
wiped out for a few months!
So tell me how you are doing?
Ralph
--