[TheForge] Welding advice needed pronto

Ralph Sproul brhlbsmt at mcttelecom.com
Tue Feb 22 19:18:58 EST 2005


Craig,  Straight argon with Mig (which Jeff will be using)? or are you
refering to Tig?

Ralph

----- Original Message -----
From: "Craig Schaefer" <craig.schaefer at verizon.net>
To: "Barking Crow" <mail at barkingcrow.com>; "Sponsored by ABANA"
<theforge at mailman.qth.net>
Sent: Tuesday, February 22, 2005 6:04 PM
Subject: Re: [TheForge] Welding advice needed pronto


> My thought is that unless you work really cheaply, he'd be better off
> buying a new/used version of what he wants.
> You can use straight argon for stainless.
>
> CraigS
> Gresham, OR
>
> Barking Crow wrote:
>
> >Here's my dilemma.  A friend that I sometimes work with on remodeling
jobs
> >wants me to turn an old 3 compartment stainless steel stand alone sink
from
> >a restaurant that we've done a bunch of carpentry work in, into a two
> >compartment sink by cutting inside both walls of the middle compartment,
> >discarding the middle section and welding the two end compartments back
> >together to make a two compartment sink with an inch and a half or so
piece
> >in the middle.  It seems to me like an incredible amount of work and that
we
> >should just cut out side one of the walls of the middle compartment and
make
> >it a two compartment sink that way.  He's worried that doing it that way
we
> >loose the nice curled top edge and that I should be able to weld the
pieces
> >back together.  Seems to me that there will be warping problems, and set
up
> >problems not to mention the grinding and rewelding trying to make the
joints
> >look nice, and the rust problems that will show up.  I'd be jusing my mig
> >with I don't remember what gas that I have for welding stainless.
> >
> >Any thoughts?
> >
> >Thanks in advance.   Jeff in Tallahassee where it hit 80 and i was hot in
> >shorts.
> >
> >
> >_______________________________________________
> >Manage membership or unsubscribe at:
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login:  blacksmithblacksmith at hotmail.com
> >password:  anvil
> >___________
> >
> >
> >
> >
> >
> >
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is