[TheForge] Chisels
Michael Horgan
lughaid at earthlink.net
Fri Feb 18 23:00:05 EST 2005
Get hold of Roger Degner and pick up a couple of the UMBA
Tapes/DVDs, There are a couple of nice videos of George Dixon demos where
he goes into making and using chisels and tooling for repussee ... looks
like he mostly uses O-1 and S-1.
At 01:33 PM 2/18/2005, you wrote:
>Does any know of a source for information on making chisels? I need to know
>which material is best for hot and cold chisels, repousse' and chasing
>chisels and how to temper the ones that need tempering. I would like to do
>an article for our newsletter but am woefully ignorant on this subject.