[TheForge] mailbox
Steve Smith
sos at alum.mit.edu
Fri Feb 18 22:00:54 EST 2005
Ours got whacked. What I did was build a cage around it. I made it in
the outline of a Conestoga wagon top. Upside down U hoops front, two
center ribs and rear (out of 5/8" 1080, which I happened to have a lot
of), the rest of the outline built out of 1/4x1/2, shaped like the sag
of the canvas. Sorry I don't have a picture.
Wasn't wrought except for the bends, arc welded together. It looked
fairly nice when done. I painted it black for the stealth effect at night.
Steve
Walter Mullett wrote:
> Well, my mailbox took a hit again last night. This happens about once every
> two months. I think it's a neighbor that I had a run in with. I wish I
> could catch him but my house is 500' off the road and hidden from that area.
>
> Rather than buying new every time, I've got two boxes that I've been
> swapping when they get bashed and straightening them back up using my sheet
> metal tools. I replaced the cheap plastic handle and clasp with forged
> ones. I've got a new molded plastic unit in the barn but I really hate the
> look of these and if the vandal can smash this one, it wont be repairable.
>
> Usually the idiot just smashes the box down it the middle. Probably uses a
> bat. This time he hit it full width and blew the back partway off.
>
> Looks like it's time to come up with a nice design in steel. I just don't
> want a clunky welded up box.
>
> Walt
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list