I have made many chasing punches from mild steel and using SQ. Otherwise, W1 (1095) is the best IMO. Simple tool steel with simple and predictable HT. If you want to get fancy for hot work tools, H13 is a very good choice. _______________________________________________ Andy 1095 is W1? I thought they were different fish. Dan Scheid