Phil wrote: > Mounted in what? > > The only two failed Centaur fire pots I've ever seen: > > 1. Mounted in a brick forge, hole burned thru it, no > ventilation. > > 2. Mounted in a steel forge, over watered, cracked. Mounted in steel. Never watered.