[TheForge] Effective filing

Mike Linn bamablacksmith at comcast.net
Fri Feb 4 22:02:44 EST 2005


Ive got several files designed for filing Aluminum and I havent had any 
problem with them clogging.

mike



At 01:48 PM 2/4/2005, you wrote:


>Ries Niemi wrote:
>>On Friday, February 4, 2005, at 11:03 AM, Dan Tull wrote:
>>
>>>Andy,
>>>Having taken Peter Ross's filing class..........
>>>I asked him what they used for a "file card"( the brush used to keep 
>>>teeth clean)
>>>that we were instructed to use since high school shop class.
>>>The reply was "We don't use one.""Don't overload the file , and it won't 
>>>clog."
>>>Let the tool work.
>>>
>>Thats all well and good, assuming all you ever file is steel.
>>But with aluminum, and some bronzes, you still need a file card.
>>They wouldnt make file cards if they werent good for something.
>
>         Yes, aluminum is the worst in terms of loading, that is for sure. 
> We aren't machines, so having a card hand can't hurt, but still endeavor 
> to develop skills such that cards are seldom needed.
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  blacksmithblacksmith at hotmail.com
>password:  anvil
>___________
>


            Mike Linn
      Artist Blacksmith
          McCalla, AL
        AFC Webmaster
http://afc.abana-chapter.com

______________________________________________________________________

"Many of life's failures are people who did not realize how
   close they were to success when they gave up. "
   ~ Thomas A. Edison
______________________________________________________________________








More information about the TheForge mailing list