[TheForge] Gas Forge Plans

Justin Fellenz sunironworks at yahoo.com
Thu Dec 29 16:29:32 EST 2005


Nice work, Larry. Clear instructions, not intimidating at all. Wish I'd
read this before I decided to figger it all out myself.

JRF

> Larry Zoeller wrote:
> 
> > To All,
> > I just posted some online plans to build an atmospheric gas
> forge,that it
> > is a really easy to build forge.  I would really appreciate it if
> you could
> > look at the plans and tell me what you think.  I would welcome any
> feedback
> > about them.  The URL is
> > http://www.geocities.com/zoellerforge/simplegasforge.html
> > 
> > Thanks in advance,
> > Larry Zoeller
> > 4312 Lahnna Dr.
> > Louisville, KY 40216
> > zman59 at earthlink.net
> > http://www.geocities.com/zoellerforge/
> > 
> > _______________________________________________
> > Manage membership or unsubscribe at:
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  blacksmithblacksmith at hotmail.com
> > password:  anvil
> > ___________
> > 
> > 
> > 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 



More information about the TheForge mailing list