>> For those following the saga of the broke cast iron post drill part:
>> Over the weekend I got started forging a replacement part. (Only had
>> a couple of hours in the shop, so I didn't get it finished.) My plan
>> is to try brazing the original after I get the replacement finished.
>>
>> Aubrey
>
>
> Way too cautious! :-)
>
>
I will try to weld it first. If I cant get a good weld then I punt and
braze it. You can always brazeup a failed weld on cast, but you can't
weld it after an unsuccessful braze....
Charles