[TheForge] Brooms and Welding Cast

Tod Estes blacksmith at atlasok.com
Sat Dec 10 08:49:37 EST 2005


Hi Aubry,
If I had my choice of brazing vs torch welding I would torch weld. Less
induced stress, more durable.
> Lousy welder eh Aubry?
>
> Kind of reminds me of what the horse trainer said about straightening out
> a
> problem horse. His cure, "Wet saddle blankets."
>
> In your case, there's nothing wrong with your welding skills burning rod
> won't cure. It's just like anything; given the basic eye hand coordination
> to hold the tools properly, everything else is knowledge and practice.
>
> Frosty
> ------------------------
> If it ain't forged
> it ain't real.
> Wrought iron is.
> The FrostWorks
>
> Meadow Lakes, AK.
>
>
> From: "Washington, Aubrey O." <awashington at ou.edu>
>
>
>
> I'm actually better at gas welding than arc welding on small things.  I
> would like to think it's because I only have an A/C welder, but secretly I
> know I'm just a lousy welder.
>
> Okay, so let's assume I'm going to use the O/A torch for this repair.
> What
> are the relative merits of brazing vs. gas welding with cast iron rod?  In
> use, this piece can be under quite a bit of stress.
>
> Aubrey
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


Tod Estes
Oologah Smithy
Oologah,Oklahoma. (Home of Will Rogers.)
Saltfork Craftsmen ABA, ABANA
Time enough for sleep in the grave.

"Prometheus: I took from man expectancy of death.
Chorus: What medicine found'st thou for this
        malady?
Prometheus: I planted blind hope in the heart of
           him.
Chorus: A mighty boon thou gavest there to man.
Prometheus: Moreover, I conferred the gift of fire
Chorus: And have frail mortals now the flame-
        bright fire.
Prometheus: yes, and shall master many arts
            thereby."



More information about the TheForge mailing list