I had forgotten about the chisel. Glad you find it useful. For anyone
that is curious all I do with H13 is forge it to shape, grind an edge,
then heat back above forging heat and let air cool. I have heard some
more detailed techniques but I have had good luck. It is great stuff.
Bob
__
On Dec 9, 2005, at 7:04 PM, Jerry Frost wrote:
> Thanks Bob:
>
> We ran too long, 45 minutes for a 30 minute show is a bit much. Quique
> and I are getting a reign on it though, 003 is around 34 minutes,
> including closing music. We're discovering we need to keep a pretty
> tight subject focus to keep to schedule.
>
> So, how about letting Quique and I grill you about working H13? I know
> there're lots of folk who'd like to know how to do it right. No
> pressure but we'd love the interview.
>
> I use the chisel you gave me for hot slitting and it works super. One
> of these days I'm going to cut it into a couple shorter lengths and
> make a couple more.
>
> Frosty
> ------------------------
> If it ain't forged
> it ain't real.
> Wrought iron is.
> The FrostWorks
>
> Meadow Lakes, AK.
>
>
> From: <schade at acegroup.cc>
>
>
>> neat. I listened to about half of show 002 so far. No problems.
>>
>> Bob
>> __
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list