Good anvil I use mine daily for 15 years and only has a few dings in it. It
is heavy enough to do a lot of work and the horn is not a bad shape for
blacksmith work more round unlike a lot of shoe'n anvil that the horn is an
oval
Dan Scheid
I have a line on a JHM Journeyman anvil (125) for $250 that has never been
used (guy decided he didn't like shoeing). Is this a good quality anvil
that could be used for smaller decorative artistic type stuff? Can a
farriers anvil be used for other stuff or is it too job-specific?