[TheForge] eucalyptus charcoal

kevin donahoe flyinpig at go-concepts.com
Sat Aug 20 05:52:20 EDT 2005


about 2%?

 -----Original Message-----
 From: theforge-bounces at mailman.qth.net
 [mailto:theforge-bounces at mailman.qth.net]On Behalf Of Peter Fels And
 Phoebe Palmer
 Sent: Saturday, August 20, 2005 4:00 AM
 To: Sponsored by ABANA
 Subject: Re: [TheForge] eucalyptus charcoal


 Just how much carbon do they stuff into those pigs anyway?

 schade at acegroup.cc wrote:
 > At the Nucor website
 > http://nucor.com/enviropages/articles/03-RenewableCarbonSource they show
 > the "Net Loss to the Environment" as 1.1 tons of CO2 per ton of Pig Iron
 > using eucalyptus charcoal. v. 2.2 tons of CO2 per ton of Pig Iron using
 > "the traditional method".
 >