>Polyethylene goes onto "warm" steel very nicely. I have a reference that suggests that the melting point of polyethylene ranges from ~90C to ~140C (~200F to ~280F), so the steel can be heated in a 250F to 300F kitchen oven and the polyethylene applied and allowed to melt onto and into the crevasses of the steel.
>
>I can attest that the result is very nice on black iron, but i haven't experimented with polished steel. I expect that some degree of skill would be needed.
>
>