Purely paraffinic (saturated) mineral oil won't "dry" (i.e., polymerize).   Unsaturated "mineral" oils should dry, but I don't know a convenient source of these, other than chemical catalogs.

There IS a work-around, though.  Polyethylene is essentially "polymerized mineral oil".  It can be melted onto a hot surface.  Works pretty well, and looks nice.  I don't know why blacksmiths don't use this more often.  It could be the answer to all those questions of protecting steel outdoors.

Bruce

>>> lance at bentoaks.org 8/15/2005 11:12:14 PM >>>
try mineral oil, clean and doesn,t turn or get sticky


 Lance


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge 
theforge mail list group photo site is
http://www.photoaccess.com 
Login:  blacksmithblacksmith at hotmail.com 
password:  anvil
___________





More information about the TheForge mailing list