The HC RR spikes are 30 to 40 points of carbon. Too soft for a decent
knife, but not bad for a light tomahawk or light adz.

Rob

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of kent
Sent: Wednesday, August 10, 2005 8:16 PM
To: forge mail
Subject: [TheForge] Forge is up!

Had a great time at the OBG meeting last Saturday; went home and fired
up the forge. Heated up some railroad spikes and a broken file, then
beat on it for a while. Drew out a tang and forged in some bevels for a
nice little knife...maybe a skinner. (LOL) It do have a bit of curve to
it, but I'll straighten it out.

Have a question for ya'll, though. What kind of steel do they use to
make railroad spikes?

Thanks,

Kent White
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list