Yes.  Some is random.  Some is quality<G>.  I've got some at home that is
good only for rebar.  I tried to make some items with it, and it shattered
where it had been hammered.  Couldn't drill through it.  Used up 4 bits
before I gave up, using good speed and oil also.

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Clyde Wynia
Sent: Wednesday, September 15, 2004 7:31 PM
To: Sponsored by ABANA
Subject: RE: [TheForge] Re: Triangles, now rebar


   >Regarding the rebar, I always thought it was trash as
>well, since a single bar had radically different behaivior end to end, 
>but as someone once told me --" That triple decker overpass over there 
>is held together by it, you really think  the melt is random?"

Here is a sight on with all the hot spit on rebar:
http://www.anvilfire.com/FAQs/reb_faq_index.htm


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________




More information about the TheForge mailing list