That is the whole idea of metal prep as used in the auto business. It
forms a paintable haze that supposedly give the paint some tooth to hold
onto, as well as getting every last rust "seed" I suppose I could do
the complete job in phosphoric, but like the immediate gratification of
sandblast followed by a wipedown with metal prep before painting.
Charles
Mike Spencer wrote:
>I think
>the acid would have purged the rust pits and the phosphate residue
>would have protected them.
>
>Now I'm going to try damming the rusted areas and pickling or maybe
>eletro-pickling just those areas. The hope is that the acid will get
>into the tiny pits that eluded the glass bead and that subsequent
>gunblue will even out the color.
>
>
>
>- Mike
>
>
>