The problem with most tire shrinkers I have seen are they but very nasty
bite marks in the steel outside of the upset. This was fine in a tire
as it was on the inside hidden by the wooden wheel but would be very
unsightly in a picket.
Roger R Degner
-
Subject: [TheForge] Upsetting the middle of a bar
I've got several tire shrinkers that would probably do this but I have
yet
to try any of them. The one that would probably have worked great is a
Star
tire upsetter/axel welder. This was used to weld stub axels to the main
axel. It has two tables with dogs that lock the stock in place with the
heated section in-between. Then with what looks like a ship's wheel
that
you turn, you compress the two tables together. I still have not got
this
machine fully freed up and working.