[TheForge] angled tenons

Wayne Ackman LongHollow.Forge at starband.net
Tue Oct 26 19:13:48 EDT 2004


You know I thought about that.  Turns out I was putting a 3/8 tenon on a 
   half inch bar so the idea of an offset becomes abit redundant anyway. 
  The rest of Darrell's suggestion worked like a champ.  They turned out 
well.

Wayne

Schade wrote:
> How to make an angled tenon?
> 
> Try to make a straight tenon. Works for me.  ;-)
> 
> Bob