In theory it's possible to do it with heavy plate, but it's much more
difficult than it appears.
A related technique is to shrink heated lines, either on one surface or
both...also tapered strips.
I tried to do it with a 1" pavement plate ( lots of hidden stresses)
and wasted a whole lot of gas ..and made a mess...finally gave up.
It was frustrating fiery fun though.....Pete F
debmiller at fuse.net wrote:
>Fire and water is the answer.
>
>I have watched trained guys straighten beams, plates, etc using a rosebud toch and a bucket of water. Kind of like a REALLY, REALLY large shrinking hammer.
>
>I am sure there are probably some process description on the internet.
>
>In basic terms it was a matter of heating the opposite side and then cooling with water and shrinking the "dimple".
>
>Ray
>Cincinnati
>
>
>
>>From: "Gladish Family" <gladish at cnw.com>
>>Date: 2004/10/15 Fri AM 09:56:35 EDT
>>To: "Sponsored by ABANA" <theforge at mailman.qth.net>
>>Subject: [TheForge] scrap plate steel
>>
>>Is there a way to straighten steel plate?
>>
>>I need to extend a welding table, so went to the local supplier and priced a
>>new 4x5, 1/2". For new steel it's ninety-some cents a pound, about $350...
>>But wait! There's a four by five chunk of 1/2" out back! About $100.
>>Unfortunately it must have had something sitting on it, because it's dished,
>>oh, maybe 3/8. Not that much, but the point is to have a dead flat surface
>>to do layout.
>>If it weren't so thick, I'd just build the frame and plug weld it, force it
>>to be straight, but 1/2" seems too burly.
>>Thanks for any suggestions,
>>Andy g.
>>
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: blacksmithblacksmith at hotmail.com
>>password: anvil
>>___________
>>
>>
>>
>>
>>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
>
>
>
>
>
More information about the TheForge
mailing list