Whats best for making steels for flint & steel kits?
Spring steel (1045 or so) quenched in oil
File steel (1095) quenched in oil
Mild steel quenched in water
some alloy like H13 or S7?
I dont have time to try everything and find the best, plus I figured
someone else has already done the experiment.
I dont want to reinvent the wheel but I need to know what material makes
the best fire steel.
thanks.