[TheForge] Hydraulic Cements etc
Woolley
wjande at erols.com
Wed Nov 10 21:34:47 EST 2004
Don,
How long does this material take to set? Where did you buy it? Thanks.
Regards,
Bill Woolley
PlumDon at aol.com wrote:
>
>In a message dated 11/10/2004 11:16:30 AM Eastern Standard Time,
>wjande at erols.com writes:
>
>Just wondering what everyone is using these days to set rail posts etc
>into cement and various masonry.
>
>
>I recently used Polygem, Inc Liquid Concrete Repair. It is an epoxy based
>product that comes in a 10oz cartridge. You mix in cartridge and discharge with
>any caulking gun. It is nearly a liquid gel when mixed and flows into every
>nook and cranny. I used it to anchor 1" square column supports in marble for
>some 200 pound gates. Pricey at around $10/cartridge but it is very, very
>tough. I put one in wrong and it took hours to chip out flake by flake...like
>knapping flint. You can dust the top with marble or concrete or whatever and
>it blends pretty well. Once in place the rails or posts are virtually
>immovable.
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
>
>
>
>
>
>
More information about the TheForge
mailing list