Bob,
It doesn't work harden. It has a better temperature range for the
working product than steel.
Jerry
At 08:12 AM 11/7/2004, you wrote:
>I've never tried 'pure iron'. I did try to buy some at LaCrosse a
>couple of years ago but all that the guy had was like 1/8"x 3/4".
>This size material is already pretty easy to forge.
>
>If the stuff is as easy to forge as everyone says you could save
>yourself some inventory by only stocking larger sizes. They
>could then be forged down for a project. It seems like 3/4"
>square/round, 1/2"x1"flat, 1' square/round, would cover most small
>shop purposes.
>
>Bob
>___
>
>
>
>
>On Nov 6, 2004, at 5:50 PM, Mark Williams wrote:
>
>>I'm interested in square and round rod, but not in very large quantities.
>>I'd like to learn more.
>>
>>Mark
>>Snow Hill, Maryland
>>----- Original Message ----- From: "Rome Hutchings"
>><rome.hutchings at theprairieismygarden.com>
>>To: <theforge at mailman.qth.net>
>>Sent: Thursday, November 04, 2004 9:23 PM
>>Subject: [TheForge] Possible return of Pure Iron to the USA
>>
>>
>>
>>Anyone who got their hands on this material knows how wonderful it was to
>>work with. But, just
>>like many a good thing........the east coast importer stopped bring it to
>>the USA. While it is true
>>that it was expensive, but the ease of working with it more than made up
>>for the cost in reduced
>>forging time.
>>
>>If there are enough people out there interested, the possibility of
>>importing it are very good. Right
>>now I have standing pre-orders for 5,000 lbs. What needs to happen is
>>this number has to be more
>>like 20,000 lbs in order to get a break on the shipping.
>>
>>So, if you are interested, please reply and pass this message on to
>>others who might be interested.
>>
>>In the mean time, check out the link: http://www.pureiron.com/
>>
>>Regards,
>>
>>
>>
>>Rome Hutchings
>>The Prairie Forge
>>13633 Ferman Avenue NW
>>Clearwater, MN 55320
>>(763) 878-1694
>>rome.hutchings at theprairieismygarden.com
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: blacksmithblacksmith at hotmail.com
>>password: anvil
>>___________
>>
>>
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: blacksmithblacksmith at hotmail.com
>>password: anvil
>>___________
>>
>>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
>
>
More information about the TheForge
mailing list