[TheForge] Smallest anvil...
Bruce Freeman
FREEMAB at pt.fdah.com
Tue May 11 12:20:59 EDT 2004
All of this strikes me as harmless insanity. But, then, what more apt
description could there be of art?
Bruce
NJ
>>> osan at netlabs.net 5/11/2004 12:05:04 PM >>>
Bruce Freeman wrote:
>
> You don't need a #80 drill. Just make a spade bit from a needle or
> (wire) cat whisker.
I sank the hardy hole last night. It's about 0.010" square.
Did it with a reground needle; all my square jewelers files
were too big, and most of them are pretty small.
I may forego the pritchel as the heel cracked doing the
hardy, so I may not want to tempt fate that my welding job
was good enough.
>
> So you gonna cast these little jobs in solid gold and solder them to
> silver buttons to wear at ABANA 2004?
The tiniest one I will do in palladium white gold, methinks.
The rest in sterling. The metals are far too costly now. I
recently finished an engagement ring for a client in SF; 15%
iridium alloy of platinum - 17 dwt. cost me over $700! Plat.
was going over $900/ozt. that day. a couple months ago it
was at $400 and change. Oddly, iridium has gone from about
$1K/ozt. to about $80, back where it was about 10 years ago.
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list