> Is it really the hardness or carbon content of the steel that changes > the tone or is it the shape? Both. Anything that makes it vibrate differently makes it sound different, by definition. Look at any musical instrument- the materials affect the tone as much as the construction does- same with any bell. You can make a bell out of a bar of soap, but it probably won't sound as good as a bronze one. Andy G.