Made a few triangles - I found that mild steel works
fine, but you get a much better ring if you quench the
corners in superquench. Really improves the tone and
intensity.
FWFaller
--- "Michael H. Murphy" <[email protected]>
wrote:
> I use half-inch round hot-rolled mild steel. 3/8
> square does a good job,
> too. I made one out of a spring, and it sounded
> real good, but
> straightening out a coil spring just wasn't worth
> it.
>
> Mike Murphy
>
> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]
> On Behalf Of Woolley
> Sent: Friday, April 30, 2004 7:09 PM
> To: [email protected]
> Subject: Re: [TheForge] Triangles
>
> What kind of steel do you use to make your
> triangles?
>
>
> Michael H. Murphy wrote:
>
> >I make one with four sides. There is an eye
> punched in the corner opposite
> >to the open corner, which has a string through it
> to hang the four-sided
> >triangle(I call 'em dinner bells) from. Regular
> three-sided dinner bells
> >should have the opening on one of the bottom
> corners. I've tried it both
> >ways, and it works better that way.
> >
> >Mike Murphy
> >
> >-----Original Message-----
> >From: [email protected]
> [mailto:[email protected]]
> >On Behalf Of Rich Maynard
> >Sent: Thursday, April 29, 2004 5:41 PM
> >To: [email protected]
> >Subject: RE: [TheForge] Triangles
> >
> >Good point. And with one being twice as long as the
> other, they should be
> an
> >octave apart.
> >
> >Rich M.
> >
> >
> >
> >>-----Original Message-----
> >>From: [email protected]
> >>[mailto:[email protected]]On Behalf
> Of Michael Horgan
> >>Sent: 29 April 2004 23:35
> >>To: [email protected]
> >>Subject: Re: [TheForge] Triangles
> >>
> >>
> >>Usually down in a corner. This gives you two
> different lengths of steel
> >>ringing, making a pleasing chime tone. Try one
> both ways and listen, see
> >>what you think.
> >>
> >>At 12:12 PM 4/29/2004, you wrote:
> >>
> >>
> >>>Should the opening on a triangle that you ring be
> up next to the eye or
> >>>down in one of the bottom corners?
> >>>
> >>>Keith "Sparky" Holmes
> >>>
> >>>
> >>Michael D. Horgan , [email protected]
> >>http://members.aol.com/lughaid/
> >>posting from
> >> A BRAZEN FORGERY
> >>Blacksmithing and Metalwork
> >>Claremont, Ca.
> >>
> >>
> >>_______________________________________________
> >>http://mailman.qth.net/mailman/listinfo/theforge
> >>theforge mail list group photo site is
> >>http://www.photoaccess.com
> >>Login: [email protected]
> >>password: anvil
> >>___________
> >>
> >>
> >>
> >>
> >
> >_______________________________________________
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login: [email protected]
> >password: anvil
> >___________
> >
> >
> >_______________________________________________
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login: [email protected]
> >password: anvil
> >___________
> >
> >
> >
> >
> >
>
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post
> was in HTML
> or had an attachment. Attachments are not allowed.
> To learn how
> to post in Plain-Text go to:
> http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
=====
Frederick W. Faller
Shiloh Forge Ironware http://users.rcn.com/ffaller/SFI_web.htm
www.immerland.com
__________________________________
Do you Yahoo!?
Win a $20,000 Career Makeover at Yahoo! HotJobs
http://hotjobs.sweepstakes.yahoo.com/careermakeover