Burch wrote: > > You may have better luck with a technique called "tig brazing". You don't > melt the base metal so there is less distortion. I've never tried it on > copper however. You could use the same copper as filler. I think that is what I was referring to. Didn't know the parents didn't melt. Learn something new every day.