That is the process, I believe the rig I saw was by All State
Larry
At 06:36 AM 3/18/2004 -0800, you wrote:
>Sounds like a setup for flame spraying. Was there something different
>about this torch that I'm just not getting from the account you
>included?
>
>Larry and Pat Brown wrote:
> >
> > Back to blacksmithing? ;-)
> >
> > I saw this system demonstrated a while ago and it is real slick. The guy
> > admitted there is a limit to how thick a piece it will work with, but he
> > wouldn't specify. Next time I see the demo I have more questions. It did a
> > great job on manifolds, etc. The powder refills are pricey also so if you
> > couldn't sell the repairs at a decent price it would take a while to recoup
> > your monies.
> >
> > On the wish list
> >
> > L Brown
> >
> > At 10:18 PM 3/17/2004 -0800, you wrote:
> > >To-day I witnessed a demonstration on building up cast iron with a Ni
> > >spray.A torch is the method of delivery. A bottle of Ni (nickel)was
> > >screwed into this custom set-up.
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________