> Agreed Bill:
>
> The serious side of this thread has indeed been about hardening a brass
> spring not tempering one.
>
> Tempering is a controlled softening of a material and is indeed most common,
> metallurgically, applied to steels. There are other materials needing
> tempering in the correct sense of the term, glass for one.
>
> Of course if someone asks THIS list about tempering glass they deserve what
> they get. <grin>
>