[TheForge] spring temper for brass question
magichammer
[email protected]
Wed Mar 10 21:25:00 2004
...not...
----- Original Message -----
From: "Bruce Freeman" <[email protected]>
To: <[email protected]>
Sent: Wednesday, March 10, 2004 2:08 PM
Subject: Re: [TheForge] spring temper for brass question
> Is the originator of this inquiry on this list or not?
>
> I would think that a brass spring would have to get its resiliency from
> work-hardening. "Tempering" per se, applies only to carbon steel.
>
> Bruce
> NJ
>
> >>> [email protected] 3/10/2004 10:15:18 AM >>>
>
> (from another list)
> Hi,
> I want to know how to spring temper light gauge brass strips.
> I know it is yellow brass (260), but I don't know if the spring temper
>
> comes from heat trating or if it is a special alloy.
> Any help would be greatly appreciated.
> Thanks!
> Kevin
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>