Oh, yeah.  For those of you that use light bulbs for keeping moisture out of
welding rod, etc.  Try coffee cup warmers.  I got mine at Walgreens for bout
$6.  Simply a 25W resistence heater and never burns out.  Had mine in my
welding rod refrigerator and Paint refrigerator for about six years now,
(and my gun safe, too).  Still puttering along, keeps the paint from
freezing in the winter and cooks the welding rod at a steady rate.

Kevin

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of magichammer
Sent: Tuesday, March 09, 2004 11:37 PM
To: [email protected]
Subject: Re: [TheForge] Spring cleaning


I change my compressor oil once a year. I use high priced synthetic
motor oil in them. Also drain the water every day. (Gulf Coast you know)
Keep a bulb in the hot box for abrasives and welding rods, vacuum the
whole shop once a week, water the flowers and that about does it.
dave m

----- Original Message -----
From: "Shannell Sugrue" <[email protected]>
To: <[email protected]>
Sent: Tuesday, March 09, 2004 7:07 AM
Subject: Re: [TheForge] Spring cleaning


> Ive wondered about changing the oil in my compressors every few years,
> operating a kinyon hammer is hard work for a compressor if you ask me but
> Ive never heard of people changing oil filters or oil in a compressor.
Does
> the mineral oil not break down as does engine oil because there is very
> little heat generated compared to an internal combustion engine. No carbon
> buildup in the oil either I guess. Does anyone change their compressor
oil?
>
>
> ----- Original Message -----
> From: "Dan Tull" <[email protected]>
> To: <[email protected]>
> Sent: Tuesday, March 09, 2004 11:46 AM
> Subject: Re: [TheForge] Spring cleaning
>
>
> > Blow out the liner hose on the mig1
> > dan tull
> > georgia
> > abba, afc, S.C. psba, obg,sofa
> > ----- Original Message -----
> > From: "Kevin Donaho e" <[email protected]>
> > To: "Theforge" <[email protected]>
> > Sent: Monday, March 08, 2004 8:11 PM
> > Subject: [TheForge] Spring cleaning
> > >
> > > What do you all do to keep things running smooth in your shop?  I sure
> as
> > > hell could have benefitted from blowing out the ol' Hobart several
years
> > > ago, though I certainly never need to weld with 3/16" rod, It's nice
to
> > know
> > > now that I can, ha!
> > >
> > > Kevin Donahoe
> > > Flying Pig Forge
> > > Morrow, OH 45152
> > > flyinpig
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________