> I'm going to be building a set of benches and anvil stand in the back of a
> fellow farrier's cube van. The box is simply 1/4"-5/16" fiberglass
panels.
> My thought was to build an angle iron frame that would bolt to the
> fiberglass walls, weld the benches to the frame and bolt them to the
floor.
> Then have horizontal angle iron trusses between the wall frames to
rigidify
> the structure port-starboard.
>
> The box is very rigid, but I'm concerned about drilling through the
> fiberglass wall and creating a bloody mess of fuzzy runners. Any ideas on
> how to poke holes in fibrglass?
>
> Kevin Donahoe
Drill a smaller hole than you intend to use, then run a heated punch through
it, to seal the fuzzies and get the hole full size. DON'T breathe the fumes-
you might try it on a bit of scrap first.
Saint Phlip,
CoDoLDS
There is only one basic human right, the right to do as you damn well
please.
And with it comes the only basic human duty, the duty to take the
consequences. -- P. J. O'Rourke