I have something to do this, but not sure where it is among my endless litany of information. If you can calculate the volume, steel and iron are about .283#/cu. in. "Mark A. Pesetsky" wrote: > > I am looking for a calculator that will give me the weight of a given size > piece of steel. Does anyone know of such a source? > > Thanks > Mark