For most things (steel) I just use 0.3 pounds per cubic inch. For aluminum
0.1 pound per cubic inch. For shapes (channel, I beams etc.) I look in a
suppliers catalog which almost always shows weight per foot.
Dave
----- Original Message -----
From: "Mark A. Pesetsky" <[email protected]>
To: <[email protected]>
Sent: Thursday, March 04, 2004 7:23 PM
Subject: [TheForge] Weight Calculator
> Here it is:
>
> http://www.metal-4u.com/prcalc.html
>
> Mark
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>