I'm not really sure what the exact temperature is, but when the brass comes
off the brush onto the steel without discoloring, that's the right heat.

BTW, wouldn't you say that any heat from about 150 up to where you can see
it glow could be defined as a "black heat"?



> -----Original Message-----
> From: theforge-bounces at mailman.qth.net [mailto:theforge-
> bounces at mailman.qth.net] On Behalf Of Darrell
> Sent: Sunday, June 13, 2004 7:24 PM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] Copper Brush
> 
> 1075 Deg F. = Dark cherry
> 1050 Deg F. = Blood red
> 900 Deg F. = Faint red
> Less than 850 Deg F. would qualify as Black heat
> Darrell
> 
> http://www.machinemaster.com
> ----- Original Message -----
> From: "northwoods" <northwoods at ez-net.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Sunday, June 13, 2004 10:44 AM
> Subject: Re: [TheForge] Copper Brush
> 
> 
> >
> > ----- Original Message -----
> > From: "Darrell" <dgehlsen at earthlink.net>
> > To: <theforge at mailman.qth.net>
> > Sent: Saturday, June 12, 2004 12:06 PM
> > Subject: Re: [TheForge] Copper Brush
> >
> >
> > > Black heat is just what it says. It is that heat that most often burns
> the
> > > blacksmith. There is no red showing but it is hot enough to cause a
> bad
> > > burn.
> > > Darrell
> >
> > Mr. Darrel, a black heat is not simply no red showing but hot enough to
> burn
> > you. It's approx. 1000 degrees, no red showing in daylight but faintly
> red
> > in the dark.
> >
> > T. Clark
> > Northwoods Forge
> >
> >
> > _______________________________________________
> > Manage membership or unsubscribe at:
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  blacksmithblacksmith at hotmail.com
> > password:  anvil
> > ___________
> >
> >
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 




More information about the TheForge mailing list