[TheForge] Copper brush

K Donahoe flyinpig at go-concepts.com
Sat Jun 12 06:02:58 EDT 2004


Arnar,

That's the temperature below which the iron shows a red color, 600*-1000* F
or so.

Kevin Donahoe
Flying Pig Forge
Morrow, OH 45152
flyinpig at go-concepts.com

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Arnar Haugedal
Sent: Saturday, June 12, 2004 4:16 AM
To: theforge at mailman.qth.net
Subject: [TheForge] Copper brush


Excuse me  -  I  am not familiar with the english word  "black heat"  -
what temperature is that?

Arnar Haugedal  (Norway)