Use a piece of copper electrical wire (cable?) as in "el cheapo extension
cord".

Strip the insulation back and frizz the end a little. Use like a brass
brush.

If you want a bigger brush, twist as many pieces together as it takes.

Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.


----- Original Message -----
From: "Larry Zoeller" <zman59 at earthlink.net>
To: "theforge" <theforge at mailman.qth.net>
Sent: Thursday, June 10, 2004 7:03 PM
Subject: Re: [TheForge] Copper Brushes


> Dan,
> That is what the ad claimed, that it would work just like a brass brush. I
> remember a while back either Mark or Mike Linn said that you could put
> copper filings on hot metal and it would make like stars on it.
>
>
> Larry Zoeller
> zman59 at earthlink.net
> Why Wait?  Move to EarthLink.
>
>
> > [Original Message]
> > From: Dan Tull <dantull at numail.org>
> > To: Sponsored by ABANA <theforge at mailman.qth.net>;
<zman59 at earthlink.net>
> > Date: 6/10/2004 9:00:00 PM
> > Subject: Re: [TheForge] Copper Brushes
> >
> > If you brush iron at a black heat, does it turn copper colored like
brass
> > does?
> >
> >
> > dan tull
> > georgia
> > abba, afc, S.C. psba, obg,sofa
> > ----- Original Message -----
> > From: "Larry Zoeller" <zman59 at earthlink.net>
> > To: "theforge" <theforge at mailman.qth.net>
> > Sent: Thursday, June 10, 2004 9:29 PM
> > Subject: [TheForge] Copper Brushes
> >
> >
> > >
> > > To All,
> > > A while back I saw an ad in one of the Chapter newsletter for copper
> > > brushes and I am making a lot of leaves right now and I would like to
> try
> > > using a copper brush instead of a brass brush.  I can not find what
> > > newsletter it was in so if anybody has any information about who is
> > selling
> > > them I would appreciate if you could pass the information on to me.
> > >
> > > Thanks in advance,
> > > Larry Zoeller
> > > zman59 at earthlink.net
> > > Why Wait? Move to EarthLink.
> > >
> > > _______________________________________________
> > > Manage membership or unsubscribe at:
> > > http://mailman.qth.net/mailman/listinfo/theforge
> > > theforge mail list group photo site is
> > > http://www.photoaccess.com
> > > Login:  blacksmithblacksmith at hotmail.com
> > > password:  anvil
> > > ___________
> > >
> > >
> > >
> >
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>



More information about the TheForge mailing list