[TheForge] Meteoric iron - wrap it in foil

Grover Richardson grover.richardson at gtri.gatech.edu
Thu Jun 10 09:21:48 EDT 2004


I stand corrected, somewhat<G>.  I was "assuming" that there was slag mixed
in the iron, not that the iron was high carbon.

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of MRScherm at aol.com
Sent: Thursday, June 10, 2004 8:34 AM
To: theforge at mailman.qth.net
Subject: Re: [TheForge] Meteoric iron - wrap it in foil


I respectfully disagree, if this were so, you could forge cast iron using
the 
same method.
Mike Schermerhorn

In a message dated 6/10/2004 8:17:12 AM Eastern Daylight Time, 
grover.richardson at gtri.gatech.edu writes:
    If I were to try to work it, I would first melt it in a crucible to
separate the iron from the slag.  Then, with a hunk of real metal, you can
forge what you want. _______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________




More information about the TheForge mailing list