[TheForge] Free Firebrick, Portland, OR area
Craig Schaefer
craig.schaefer at verizon.net
Sun Jun 6 11:10:18 EDT 2004
Dave,
These don't appear to be used, as they are not discolored at all. They
were originally sold by the company (not to me), so I am guessing they
didn't consider them a liability.
CraigS
Gresham, OR
David E. Smucker wrote:
>Do you know if it came from the smelting pots themselves? If so they may
>have a rather high contamination with fluorides from the smelting process
>itself. I would not use such firebrick myself. If the firebrick is new, it
>should be OK to use or if the brick came from metal transfer pots that
>should not be a problem. I am a retired mechanical engineer who spent 32
>years with ALCOA. (Aluminum Co. of America). "Spent pot lining" as we
>called them are considered a hazardous waste. This is because of the
>fluoride salts that become part of the lining in use. We (Alcoa) would not
>let spent pot lining out of our control. I don't know what Reynolds used to
>do. (Reynolds is now owned by ALCOA). On the other had we would scrap used
>firebrick from transfer pots, and melting furnaces with no issue. Surplus
>new brick would sold / scraped depending on how much someone wanted to get
>rid of.
>
>Dave Smucker
>
>----- Original Message -----
>From: "Craig Schaefer" <craig.schaefer at verizon.net>
>To: "Sponsored by ABANA" <theforge at mailman.qth.net>
>Sent: Saturday, June 05, 2004 10:57 PM
>Subject: [TheForge] Free Firebrick, Portland, OR area
>
>
>
>
>>Hey, guys,
>>I have some firebrick that I want to get rid of. It is the old brick
>>that was used to line the pots at the old Reynolds Aluminum plant. Some
>>look used, some don't and I have about 100 of them, maybe a few more.
>>Don't know what the composition is, but I put one in my gas forge for
>>about 30 minutes until it was cherry red all over. Cooled it and there
>>doesn't seem to be any degradation. I use them as a backdrop to a coal
>>forge I have.
>>Free to anyone who wants to pick them up.
>>
>>Contact me at craig.schaefer at verizon.net
>>
>>thanks,
>>
>>CraigS
>>Gresham, OR
>>
>>
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: blacksmithblacksmith at hotmail.com
>>password: anvil
>>___________
>>
>>
>>
>>
>>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
>
>
>
>
>
More information about the TheForge
mailing list