[TheForge] Cheap anvil & forge in NE Ohio
Andy Vida
osan at netlabs.net
Sat Jul 31 12:09:14 EDT 2004
"Michael H. Murphy" wrote:
>
> For what it's worth, I bought a 100-lb Vulcan anvil a few years ago --
> almost mint condition. I used it mostly for demos because I didn't want to
> carry my 276-lb Hay-Budden around. It worked real well for me, and still
> does. The edges are sharp enough to make the shoulders for nails, and they
> have held up real well. I'd like to find a 200- or 250-lb anvil that good,
> and in as good condition.
I have an absolutely pristine 106# PW. It's perfect for demos.
Even I, Mr. Wimpysmith, can lug it around with relative ease.
My 200# HB is also pristine with the exception of the tail being
broken off, but there's part of the tail to one side of the hardy
hole that remains. Turned out to be very good for small work. :)
More information about the TheForge