I need to anneal some small pieces of aluminum plate. 1/8 to 3/16 thickness. I do not know the alloy. I have oxy/acetylene at my disposal. I know that heating to 650F and air cooling is a good rule of thumb, but how do I approximate 650F with the torch? CraigS Gresham, OR > >