I suppose if you wanted to reduce it to dust first, you could get it to 
burn around 1000F


cs

Andy Vida wrote:

>Jerry Smith wrote:
>  
>
>>         Titanium has an ignition point of something like 6,000 degrees F.
>>    
>>
>
>	Titanium is very difficult to light, but once started, you do
>	not want to be anywhere near it.  It is a reactive metal, meaning
>	it has a great affinity for oxygen, among other things.  Once you
>	go past a threshold, it is like a runaway train.