Jerry Smith wrote: > > Titanium has an ignition point of something like 6,000 degrees F. Titanium is very difficult to light, but once started, you do not want to be anywhere near it. It is a reactive metal, meaning it has a great affinity for oxygen, among other things. Once you go past a threshold, it is like a runaway train.