Andy,

I have a lathe, but tapers are beyond my capibilities.

Robert Ehrenberger
Shelbyville, Mo.

++++ Original Massage  ++++
Date: Sat, 17 Jul 2004 09:39:33 -0700
From: Andy Vida <osan at netlabs.net>
Subject: Re: [TheForge] Re: Cone Question

Bob Ehrenberger wrote:

> Andy,
>
> I do have a Dake press and my son has a 25ton hydrolic press.   If I had
top
> and bottom dies I probably wouldn't have asked for advice.

If you have access to a lathe, make them.  Mild steel should
do the trick for this application.  Just a thought.